Forget electrolysis and start with gold chloride. That makes the best quality colloidal gold.Use 20ml 1% gold chloride from Salt Lake Metals.Use 1 ml of 1 Molar sodium carbonate solution per liter of water.Use 1 ml or more Karo Light corn syrup per liter.*Use 2 grams of animal based gelatin per liter.*Heat to 90C.*You will probably need to experiment with these values.
Quote from: kephra on September 20, 2018, 12:00:40 PMForget electrolysis and start with gold chloride. That makes the best quality colloidal gold.Use 20ml 1% gold chloride from Salt Lake Metals.Use 1 ml of 1 Molar sodium carbonate solution per liter of water.Use 1 ml or more Karo Light corn syrup per liter.*Use 2 grams of animal based gelatin per liter.*Heat to 90C.*You will probably need to experiment with these values.I agree ! Easy fast and great quality .